Resources are limited and recycling is unlimited. The latest news in the plastic industry, recyclable plastic must be forced to add recycled materials for secondary production, supermarket shopping bag vest bag in the production process of waste B side material will produce 15-25%, plastic bag waste side material recycling is also imperative to the environment and resource regeneration.
PLA+ PKAT + starch fully degradable film regeneration and granulation process:
Degradable film scraps can be directly into the granulator to cut, break, shrink, agglomerate, extrusion
Process temperature: 120℃-140℃
Granulation method: water ring granulation or air cooling
Moisture outside particles: ≤0.8%
Particle appearance: round and full, no bubbles
Color: white, off-white
Production: 200-600 kg/h
Regenerated particles can be directly added in the film blowing process